Dear all,

Shall we can use E7016 for root welding (open root) for s355 JR

Regards,
Jibin Philip

Mostafa Kamel Hussein

unread,
Jan 25, 2016, 8:22:49 AM1/25/16
to material...@googlegroups.com
Firstly; you should prepare WPS supporting with PQR and after passing the tessting, you decided to use it. but any way and from our experience you can use E7016 for root in your PQR or use old own WPS and then No problem to use it in production