Regarding SS 304 Cleaning

51 views
Skip to first unread message

Mohit Aggarwal

unread,
May 12, 2016, 3:12:11 AM5/12/16
to materials-welding

Dear Experts,

Kindly let me know that If SS is effected by Carbon steel and surface get little effected, then is it right to clean it with Nitric Acid by dipping.

Regards,
Mohit Aggarwal.

Jim Price

unread,
May 12, 2016, 6:12:02 AM5/12/16
to material...@googlegroups.com

Yes you can use a nitric solution for passivation to eliminate carbon pick-up.

 

Jim Price | Welding Engineer, CWI

Direct:  320.7463439 | Fax: 417-862-5564

jimp...@polarcorp.com

cid:image001.jpg@01D0E005.E9837830

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALTezPNOt0CCbV9uYQB7FC8oWU1vrx71_PgfXYnrn_Ab8kOb3w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Kannayeram Gnanapandithan

unread,
May 12, 2016, 6:34:15 AM5/12/16
to materials-welding
use 1:4, Hydrofluoric acid :Nitric acid with water and clean 

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

Abdul Rauf

unread,
May 14, 2016, 8:37:07 AM5/14/16
to material...@googlegroups.com
You can use nitric solution for passivation to remove carbon.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALTezPNOt0CCbV9uYQB7FC8oWU1vrx71_PgfXYnrn_Ab8kOb3w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
Best Regards,
 
Abdul Rauf
Lead QA/QC
BLCT-Project KSA
Cell# 00966 590 637 965

dili...@gmail.com

unread,
May 14, 2016, 11:40:06 AM5/14/16
to Abdul Rauf
What is removed by passivation is Fe and not C

Sent from my BlackBerry 10 smartphone.
From: Abdul Rauf
Sent: Σάββατο, 14 Μαΐου 2016 - 15:37
Subject: Re: [MW:24794] Regarding SS 304 Cleaning

David Harvey

unread,
May 14, 2016, 11:40:19 AM5/14/16
to material...@googlegroups.com

Stainless steel weld surfaces are invariably contaminated by the iron oxide-rich condensed fume deposits surrounding the weldment. If left in situ, this can cause very unsightly rust staining when it become damp . This is what has to be removed. There are numerous proprietary cleaners available from local welding distributors.

Sincerely,

D  Harvey, 



----Original message----
From : abdulr...@gmail.com
Date : 14/05/2016 - 13:35 (GMTST)

To : material...@googlegroups.com
Subject : Re: [MW:24794] Regarding SS 304 Cleaning

To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOoEmJ0uzzOoxEBo%3DfD9jMeMi_2JxeraXs%2BxBhAo28z4pzeYA%40mail.gmail.com.

Mehdi Vafakhah

unread,
May 14, 2016, 10:48:24 PM5/14/16
to Materials & Welding
Hi

Astm a380 and 697 could be useful.