L-300 TECHNICAL REQUIREMENTS
The qualification record must record the essential variables
for the welding process and list the ranges qualified.
While the “actual values” recorded on the test record will
be the same as for a test record prepared according to
ISO 9606-1 or ISO 14732, the ranges qualified will be different
for a record prepared according to Section IX.
Care should be taken to select material used for the test
coupon from those that are assigned a P-Number under
QW-420 and filler metals that are assigned F-Numbers
in accordance with QW-432 in order to ensure full interchangeability
with other materials that are assigned
P-Numbers or F-Numbers.
Since the forms may be in any format as long as the actual
values, ranges qualified, and test results are recorded,
a record showing the ranges qualified under both ISO and
ASME may be on separate forms or they may be on one
form at the discretion of the organization.