Hi
Is it acceptable to use plate instead of cladding for blind flange? The cladding material and plate is CU NI 90/10. 
The below drawing is the manufacturing offer.

1.jpg

Vinay Thattey

unread,
May 3, 2020, 3:33:43 AM5/3/20
to material...@googlegroups.com
Application ??

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3612b777-edba-433e-8658-cf93bc126f3d%40googlegroups.com.

Prasanta Kumar Pal

unread,
May 3, 2020, 3:58:55 AM5/3/20
to material...@googlegroups.com
You need to do design calculation with cladded material 

Baha

unread,
May 4, 2020, 7:20:11 AM5/4/20
to Materials & Welding
The application of blind flange (ASTM A105+CUNI 90/10 cladding) is for sea water


On Sunday, May 3, 2020 at 12:03:43 PM UTC+4:30, Vinay wrote:
Application ??

On Sat, 2 May 2020 at 13:55, Baha <b.ni...@gmail.com> wrote:
Hi
Is it acceptable to use plate instead of cladding for blind flange? The cladding material and plate is CU NI 90/10. 
The below drawing is the manufacturing offer.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.

Prakash Hegde

unread,
May 5, 2020, 11:31:14 AM5/5/20
to material...@googlegroups.com

Hi !
Liner attachment.is not accepted by designer ( Ask licensor)
You require to have a metallurgical bonding by carrying out overlay welding
90:10 Cu Ni.is compatable with C S

Regards
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/665ec29e-8f34-43ab-a44e-9a218ae7d23b%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages