Minimum distance between two adjacent pipeline for 8"

53 views
Skip to first unread message

Saumey Shrivastav

unread,
Dec 25, 2021, 1:44:40 AM12/25/21
to material...@googlegroups.com
Dear sir,

Kindly confirm me to technical specification for Minimum distance between two adjacent pipeline and do needful.

Thank you

Mohd Siraj

unread,
Feb 7, 2022, 4:18:30 AM2/7/22
to Materials & Welding
for min distance between with insulation as per shell, dep is 25mm.

for uninsulated pipe, refer to drawing co-ordinate for the gap.