Allowable tolerance

91 views
Skip to first unread message

Dhaneesh p

unread,
Oct 31, 2020, 10:09:22 AM10/31/20
to Materials & Welding
Dear experts 
my query is , what is allowable tolerance in length , diameter , thickness for material receiving inspection of following ( please mention reference code   )
1) pipe ASTM 312 TP 304  , SIZE 3/4" , THK : 2.87 mm , Length : 6 m 
2) fittings  ASTM A 403 WP 304 , THK : 3.38
Regards 
Dhaneesh 

Jamie Reyes

unread,
Nov 1, 2020, 5:36:35 AM11/1/20
to material...@googlegroups.com
Review the following:

ASME 36.19
ASME B16.9
ASME B16.11
ASTM A960

Cheers.....

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bda38b20-5a5b-4094-9d28-2b8a410fa53cn%40googlegroups.com.
--
Regards,
Jamie Reyes
J.R. Machine Company, Inc.

Vinay Thattey

unread,
Nov 1, 2020, 5:36:35 AM11/1/20
to material...@googlegroups.com
In general it is 12.5 %

--

venkat chikkala

unread,
Nov 1, 2020, 5:36:35 AM11/1/20
to material...@googlegroups.com
Dear,

Refer referenced documents mentioned in applicable material specification.

Regards,
CH V RAMANA 

--

Vijay Makwana

unread,
Nov 1, 2020, 5:37:25 AM11/1/20
to material...@googlegroups.com
Hell |Dhaneesh,

please refer to the respective standards itself, there everything is clearly described and you may find your own solution.
MTech (Metallurgical & Materials Engineering)
Indian Institute of Technology Kharagpur (IIT)



--

Kannayeram Gnanapandithan

unread,
Nov 1, 2020, 10:25:03 PM11/1/20
to materials-welding

Dhaneesh p

unread,
Nov 2, 2020, 4:00:23 AM11/2/20
to Materials & Welding
sir 
apart from material standard,  ASME SEC II PART A , Have guidelines for tolerance  , can i follow that  ?

Reply all
Reply to author
Forward
0 new messages