Dear expert ,
Please brief difference between low alloy steel vs high alloy steel.
A335 P9 is low or high alloy steel.
Sankaran Sp
unread,
Dec 28, 2022, 10:31:36 PM12/28/22
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Sign in to report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to Materials & Welding
Dear Mr. Mithlesh kumar,
when we adding the total alloying elements of Cr,Ni,Mo, if the total is less than or equal to 10% this is low alloy steel, total alloys are greater than 10 % that is high alloy steel.
You do not have permission to delete messages in this group
Copy link
Report message
Sign in to report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to material...@googlegroups.com
Low alloy less than 5% of individual or aggregate of total number of alloying elements , greater than 5% and less than 10.5% is medium, and above 10.5 high alloy as mentioned for low alloy.