E 7018 and E 8010-B2 IN SAME BAKING OVEN

83 views
Skip to first unread message

Aneesh K

unread,
Mar 20, 2023, 6:53:31 AM3/20/23
to material...@googlegroups.com
Hi Folks,

Could any experts clarify regarding the subject matter, if it is allowed to keep both E7018 and E 8018-B2 electrodes in the same Baking/ Holding oven for conditioning purposes.
As required by Saudi Aramco Standard SAES-A-206. section 7.7.1, """"Electrodes shall be properly stored and segregated in the store, shop, or ovens to avoid mix-up. Separate ovens are required for different welding consumable types.""""

Please clarify if E7018 and E8018-B2 are to be considered as different type of electrodes from 
Baking point of view 



Thanks and Regards

Aneesh

james gerald

unread,
Mar 20, 2023, 10:49:38 PM3/20/23
to material...@googlegroups.com
Electrode type indicates whether low H2 Basic / Cellulosic / Rutile and also includes as material type such as carbon steel / SS.

In your case, you can use the same oven.

Thanks & Regards

J.Gerald Jayakumar



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFWZHfnzJU4K%3DoHLBotqv4QVrGfKzKPakyiMvAAi2xGxMjp%3DQA%40mail.gmail.com.

P Goswami

unread,
Mar 20, 2023, 11:27:19 PM3/20/23
to material...@googlegroups.com

Hello Aneesh,

 

Technically the baking/reconditioning temperature of E-7018 & E-8018-B2 consumables are very close or may be the same. However, under shopfloor conditions  even if the consumable is segregated well in the same oven there’s every possibility of Consumable Mix Up within the same oven or welders picking up the wrong consumable unknowingly.

 

Hence to be on the safe side, it’s preferred to have separate holding ovens for E-7018 & E-8018B-2 type welding consumables as recommended by Aramco Specifications.

 

Thanks

 

Pradip Goswami.P.Eng, IWE.

Independent Welding & Metallurgical Engineering Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgos...@rogers.com,pradip....@gmail.com

Cell/Whasapp:1-905-9793232

 

On Monday, 20 March, 2023 at 04:23:26 pm IST, Aneesh K <aneesh...@gmail.com> wrote:

 

 

Hi Folks,

 

Could any experts clarify regarding the subject matter, if it is allowed to keep both E7018 and E 8018-B2 electrodes in the same Baking/ Holding oven for conditioning purposes.

As required by Saudi Aramco Standard SAES-A-206. section 7.7.1, """"Electrodes shall be properly stored and segregated in the store, shop, or ovens to avoid mix-up. Separate ovens are required for different welding consumable types.""""

 

Please clarify if E7018 and E8018-B2 are to be considered as different type of electrodes from 

Baking point of view 

 


 

Thanks and Regards

 

Aneesh

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFWZHfnzJU4K%3DoHLBotqv4QVrGfKzKPakyiMvAAi2xGxMjp%3DQA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

Aneesh

unread,
Mar 21, 2023, 12:22:36 AM3/21/23
to Materials & Welding
Hi Pradip ji,

Thank you for your prompt response.

Thanks and Regards

Aneesh 