Dear Experts, 

How to calculate consumables required in SMAW/MIG/TIG process

The welding in running meter are as below 
1800m  of IS2062 steel 8mm thick
630m of SS316L stainless steel 6mm thick
3500m of lining inside shell 2mm thick 

Are there any other dimensions required for calculations

Thank you.

masna uday

unread,
Apr 8, 2024, 11:10:21 AMApr 8
to material...@googlegroups.com
Dear greetings for the Day, 


Required Consumable formula 
W= A x e x L x 1/E
 Where, 
W= Required  quantity / Filler metal ( grams)
A = Cross section of Area ( cm2)
e= Density of material 
L= length of the weld in cm 
E= Deposition efficiency
 


A= ((rxt)+(t-f)2xtan(θ/2))/100

Where,
r = root
t = thickness
F= Foot face 


Thanks and regards, 

   


Masna Uday Kumar

Ph:9063983052

masna...@gmail.com

 



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/52f6ad61-e224-41af-ab74-4ffd1a6d897fn%40googlegroups.com.

basem elabd

unread,
Apr 8, 2024, 11:10:24 AMApr 8
to material...@googlegroups.com

--

Welding atvprojects

unread,
Apr 8, 2024, 11:10:38 AMApr 8
to Materials & Welding
Please go through for calculations link below:

This article explains steps and benefit of weld consumable calculation. Free excel for single V weld consumable calculator is also provided.


From: material...@googlegroups.com <material...@googlegroups.com> on behalf of SMM <sohil...@gmail.com>
Sent: Monday, April 8, 2024 11:32 AM
To: Materials & Welding <material...@googlegroups.com>
Subject: [MW:34852] Qty of Consumables required
 
--
Reply all
Reply to author
Forward
0 new messages