Hai everyone
I want to know the pressure vessel mill tolerance (thickness) for SA 516 GR 70 N ...which ASME code mentions the tolerance ....is it acceptable to shorten
My plate thickness is -20mm - but I got thickness is 19.6,19.7?
FOLLOWING CODE: ASME SEC VIII- DIV -01