I have an existing WPS-PQR of SMAW process with impact testing requirement. Since the PQR was done with a 38mm plate the base metal thickness qualified is from 16 to 200mm when impact testing is required. For the same job where I have to do Tack welds for the fit-ups will this WPS-PQR suffice for the tack welds? or a separate WPS-PQR will be required?

james gerald

unread,
Feb 8, 2022, 6:45:10 AM2/8/22
to material...@googlegroups.com
For Tack welds hope base metal thickness remains the same and there is no lower limit on weld metal qualified.

Thanks & Regards

J.Gerald Jayakumar




On Tuesday, 8 February, 2022, 03:30:20 pm GMT+4, Shivprasad Yadav <shivpr...@gmail.com> wrote:


I have an existing WPS-PQR of SMAW process with impact testing requirement. Since the PQR was done with a 38mm plate the base metal thickness qualified is from 16 to 200mm when impact testing is required. For the same job where I have to do Tack welds for the fit-ups will this WPS-PQR suffice for the tack welds? or a separate WPS-PQR will be required?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/067a69af-f523-4817-86ae-7c92239d9b62n%40googlegroups.com.

Mohd Siraj

unread,
Feb 8, 2022, 10:19:04 PM2/8/22
to Materials & Welding
if tack weld is merged with welding no new WPS is needed.

if tack weld is removed from base metal, then yes need new WPS to support your tack weld thickness. or else can use GTAW WPS( if u have).

Prasad rao

unread,
Feb 8, 2022, 10:19:08 PM2/8/22
to material...@googlegroups.com
Could please tell me about tack weld specficatio please

james gerald

unread,
Feb 9, 2022, 6:06:57 AM2/9/22
to material...@googlegroups.com
check B31.3

Thanks & Regards

J.Gerald Jayakumar


Prasad Talari

unread,
Feb 9, 2022, 10:16:26 PM2/9/22
to materials-welding
Hi,

your existing WPS will suffice the requirement for tack welds, separate WPS does not required

Regards
Prasad Talari
Welding Engineer

Vishwas Keskar

unread,
Feb 9, 2022, 10:16:27 PM2/9/22
to material...@googlegroups.com
WHAT IS YOUR JOB THICKNESS ?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages