welder qualifiation as per awsd1.1 using wps qualified by asme secIX

37 views
Skip to first unread message

anil kumar

unread,
Oct 24, 2015, 1:18:27 AM10/24/15
to Materials & Welding
hi I have A wps which is qualified as per ASME Section IX, my question is can i use this wps for welder qualification(welder qualification as to done as per AWSD1.1).

Mohd Azam

unread,
Oct 24, 2015, 1:48:26 AM10/24/15
to material...@googlegroups.com
No

On Fri, Oct 23, 2015 at 5:52 PM, anil kumar <anil...@gmail.com> wrote:
hi I have A wps which is qualified as per ASME Section IX, my question is can i use this wps for welder qualification(welder qualification as to done as per AWSD1.1).

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4e03f5ed-1883-40ac-a3b2-4227f4623db7%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

John Henning

unread,
Oct 24, 2015, 12:50:05 PM10/24/15
to Materials & Welding

yes = as long as "the Engineer" as defined by AWS D.1.1 accepts alternate qualification.




From: material...@googlegroups.com <material...@googlegroups.com> on behalf of anil kumar <anil...@gmail.com>
Sent: Friday, October 23, 2015 9:52 AM
To: Materials & Welding
Subject: [MW:23789] welder qualifiation as per awsd1.1 using wps qualified by asme secIX
 
hi I have A wps which is qualified as per ASME Section IX, my question is can i use this wps for welder qualification(welder qualification as to done as per AWSD1.1).

--