For long piping(Carbon steel, alloy steel), butt welding of large diameter(219mm OD TO 606mm OD, THK - 18.26mm to 42 mm )pipes is carried out. 
For PWHT of these butt welds, what are the parameters shall be considered for effective PWHT?

Alan Denney

unread,
May 26, 2015, 3:23:00 AM5/26/15
to material...@googlegroups.com

The following link may be of use to you.

http://www.twi-global.com/technical-knowledge/job-knowledge/heat-treatment-of-welded-joints-part-3-116/

 

The other articles by TWI under the same topic should also be of interest.

 

Best wishes

 

Alan Denney

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/123817e2-66c9-440c-9da6-21d6b616ce26%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


This email has been scanned by BullGuard antivirus protection.
For more info visit www.bullguard.com

Vishwas Keskar Welding Manager Pune India

unread,
May 31, 2015, 8:48:54 AM5/31/15
to material...@googlegroups.com
Alan 
thanks .We intend to follow B 31.1 POWER PIPING CODE AS FABRICATION CODE IS ASME B 31.1