You won’t find a specific para for weave width, other than ASME section 9, relating to your WPS that has been qualified. Maximum weave width shall be as stated in your WPS (welding procedure).
I believe this will be true for other Standards.
Best Regards,
Jim Price | Welding Engineer, CWI
Direct: 320.7463439 | Fax: 417-862-5564
![]()
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-weld...@googlegroups.com.
To post to this group, send email to
material...@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/757ab274-8b90-4e73-93a9-35e7c078e57f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Generally 10mm
Pls confirm that Weld weaving width , weld weave maximum how much we can accepted in GTAW process ?
--
Pls confirm that Weld weaving width , weld weave maximum how much we can accepted in GTAW process ?
--
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAK2QV3QFiqaSwxrdqcXrstoGNNThQbXqq%3D1YEt-x6G1YyPjRoQ%40mail.gmail.com.
Sec IX, has nowhere said about weaving width for any welding process, but in Section 1 and Section 8, it has given for welding by SMAW, the weaving width may be 4Xcore dia.THANKS & BEST REGARDS,KG.PANDITHAN, IWE, AWS-CWI, CSWIP 3.1,CONSULTANT-WELDING & QUALITY
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ce31dd8b-feec-4270-8bd7-1e585e4deb74%40googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFnxsQy5p%2B3g1hN7e%2BKftd8%2BqGgJs10kGL3B_2NuJJHiTWCsWA%40mail.gmail.com.
Pls confirm that Weld weaving width , weld weave maximum how much we can accepted in GTAW process ?
--
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHmEnHg8oBk8BuYiHw2U1%2B68_ri3QZ9EdgtUeT%2BfHN-YzEBdJg%40mail.gmail.com.
Nowhere found this is why you need to specify weave or stringer.
Weave width needs to be included.
Best Regards
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMhbo768T7d3h%2BJTE5BUwN-pNvMpHVSWcHA1i4hvcojVA%40mail.gmail.com.
Dear All experts,
Kindly conclude....the matter because many of us have same query for GTAW.
Thanks
Ramesh Barot
------ Original message------
From: Jim Price
Date: Tue, 5 Apr 2016 08:14
To: material...@googlegroups.com;
Subject:RE: [MW:24630] GTAW weld weaving
Nowhere found this is why you need to specify weave or stringer.
Weave width needs to be included.
Best Regards
Jim Price|Welding Engineer, CWI
Direct: 320.7463439| Fax: 417-862-5564
![]()
On what basis it is acceptable, any ref pl
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/467d2395-a259-4815-b8db-585cde441a74%40googlegroups.com.
Its depends on the PQR.
Weaving tends to increase the heat input on the material.
--