mechanical properties

58 views
Skip to first unread message

Jijo Vg

unread,
Apr 5, 2023, 2:01:50 AM4/5/23
to Materials & Welding
Hi 
I want to know which Asme class I can find the mechanical properties like hardness, elongation, hardness etc... I already searched (ss316l) in ASME SEC II Part SA-312 TABLE 4- but it only showed tensile and yield not in hardness etc...  .I have a doubt about the same p no are the mechanical properties are same for  ss 304,316,316l etc? 

Vinay

unread,
Apr 9, 2023, 11:00:14 PM4/9/23
to material...@googlegroups.com, jij...@gmail.com
It seems that Ur looking for SS304/316 pipe . Yes ASTM-A-312 does not specifically mentions about  elongation.

On Wed, 5 Apr 2023 at 11:31, Jijo Vg <jij...@gmail.com> wrote:
Hi 
I want to know which Asme class I can find the mechanical properties like hardness, elongation, hardness etc... I already searched (ss316l) in ASME SEC II Part SA-312 TABLE 4- but it only showed tensile and yield not in hardness etc...  .I have a doubt about the same p no are the mechanical properties are same for  ss 304,316,316l etc? 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/457b018f-86ad-4076-8d4c-40a8de41af7cn%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages