1. You can use it2. 309LSent from my Samsung Galaxy smartphone.-------- Original message --------From: Materials & Welding <yudistir...@gmail.com>Date: 23/03/2017 08:19 (GMT+02:00)To: Materials & Welding <materials-welding@googlegroups.com>Subject: [MW:26259] SA 387 Gr. 11Hai All,--I'm knew in this group.I believe many of you have many expereince in this situation.I've been try to looking many refferences but still hard to find the right one.my Problem are:
- with what method that I need to use when I want to Joint Plate for Type material like SA-387 Gr. 11 to SA 516 Gr. 70. and what kind of Electrode that I need to use? is it enough using ER 80S B2 in Gtaw?
- Similiar to question above, What Kind of method that I will use when want to join material Plate like SA240 Gr. 304H to SA-387 Gr. 11?
perhaps many of you can help me on this situation.Thank you for your information on thisWarm regardsYudistira
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/44bc1812-6180-4cf4-ad6f-aed21871075d%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/etalxojgifeec5qr1ff1gw9l.1490287776746%40email.android.com.