Dear Experts,

I have a doubt noted below for your advice.


If I used the Steel Designation SA 516 Grade 70  65  60 MTLTV for procedure qualification. I will be qualified for P1 G 1 / 2   To   P1 G 1 / 2
Single PQR / WPS satisfy my below welding requirements. 
(Toughness & PWHT considered)
1) SA 516 Gr.70 to SA 516 Gr.70
2) SA 106 Gr. B to SA 105
3) SA 106 Gr. B to SA 106 Gr. B

Thank You & Regards
Williams P Wilson
QA/QC Engineer
Please consider the environment before printing this message

Jenish Mistry

unread,
Nov 28, 2022, 2:35:48 AM11/28/22
to material...@googlegroups.com
Yes Definitely for PQR.

But you need Separate WPS ...

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHBxnQ6nEpnmYNSJgSUjNqO%3DM__7SFR4aa3QSfCWWaaQB_yoDw%40mail.gmail.com.

Vishwas Keskar

unread,
Nov 28, 2022, 3:51:22 AM11/28/22
to material...@googlegroups.com
Is there any requirement of Notched Toughness Requirements in the job by Design Engineering?

On Mon, Nov 28, 2022 at 8:56 AM williams p wilson <william...@gmail.com> wrote:
--

williams p wilson

unread,
Nov 28, 2022, 4:37:56 AM11/28/22
to material...@googlegroups.com
Yes, Impact Test required for the weld joints.


Thank You & Regards
Williams P Wilson
QA/QC Engineer
Please consider the environment before printing this message

Manikandan J

unread,
Nov 28, 2022, 5:10:42 AM11/28/22
to material...@googlegroups.com
P1 G1 to P1 G2 PQR allows to weld  P1 G1,G2 to P1G1, G2 Base Metals

--

williams p wilson

unread,
Nov 28, 2022, 10:14:42 PM11/28/22
to material...@googlegroups.com
Dear Sir,

My case is the test coupon plates (02 No's) are the same grade : SA 516 Grade 70  65  60 MTLTV


Thank You & Regards
Williams P Wilson
QA/QC Engineer
Please consider the environment before printing this message

Zacharias Rohith Joseph

unread,
Dec 21, 2022, 10:23:26 PM12/21/22
to Materials & Welding
Can you please explain why we need separate WPS ? 

Zacharias Rohith Joseph

unread,
Dec 21, 2022, 10:23:32 PM12/21/22
to Materials & Welding
All these are P1 materials then they should be qualified by default. 

srinivas rao

unread,
Dec 26, 2022, 1:21:00 AM12/26/22
to Materials & Welding
A single WPS will suffice this requirement , Mr.Williamns  your undestanding was correct ,
 ensure  consuambels are using  while production welding are meeting the requirment of Gr.70 plate weding in WPS as a note.
if you want to support this PQR for pressure vessels  u need  SA 516 Grade 70  65  60 MTLTV to SA 516 Grade 70  65  60 MTLTV (mostly prefered combination )- it can support for all the combinations 

in other case you can have one side it is SA 516 Grade 70  65  60 MTLTV and other side  SA 516 Grade 65 plate for plate  to pipe /flange /fitting scope (better avode this ) - some clients wants this combination also.. u can concence them with code.

Regards,
Srinivas Rao
welding Engineer 

Mohd Siraj

unread,
Feb 2, 2023, 4:06:37 AM2/2/23
to Materials & Welding
Yes, considered, you have highest impact temp. (-Ve)