Dear Expert,

I need to inspect vacuum receiver which is operating at 450 MMHG / -0.599 Bars.

Please let me know at what pressure do i need to carry out Hydrolic / Pressure / vacuum test.

Kindly do needful.

--
Thanks and Regards, ?

Mohammed Ghani,

CSWIP 3.1 / BGAS L-2 / ISO 9001:2008 QMS LA.

Mechanical Inspector,
BUREAU VERITAS.


ü
 Please consider the environment before printing this email.

 "Be the change you wish to see in the world"

---Mahatma Gandhi---

waheed

unread,
Apr 12, 2016, 10:09:37 PM4/12/16
to material...@googlegroups.com

I think it's not required to to carry out any of them unless it was in service and subject to major repairs 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG7AWVjtCr2h4b9%3D%3D-EiSpBeCPHdqw2qPgfwbnBCpe93aL_Nwg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Mohd Siraj

unread,
Apr 13, 2016, 12:07:50 PM4/13/16
to Materials & Welding
Pull the vaccuum more than design of 1.5 tine if it hold during duration it is okey.