Require explanation on resistance welding cycle attached in a fle

11 views
Skip to first unread message

Chirag Sandhane

unread,
Oct 14, 2016, 5:37:15 AM10/14/16
to Materials & Welding
Dear Experts,

                     I want your to understand attached resistance welding cycle. I want to understand meaning of squeeze time, weld time, cooling time, quench time, temper time, pulse, impulse, preweld interval, weld interval & postweld interval. How these parameters can be used in welding? What is significance of each parameter?

Thanks & Regards,
Chirag Sandhane