http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a0bf2487-921c-40df-a1f4-cc6886e07182%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Mock up qualification as per section IX with ten tubes required. Additionally pull test is to be done.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a0bf2487-921c-40df-a1f4-cc6886e07182%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3vk1jfblmfkop6qg13yd2on8.1478960138453%40email.android.com.To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Minor adjustment - ASME Section VIII Div. 1 does not mandate tube-to-tubesheet mockup for qualification - however Division 2 does.
From: material...@googlegroups.com [mailto:material...@googlegroups.com]
On Behalf Of George Dilintas
Sent: Sunday, November 13, 2016 7:28 AM
To: Meghanadh K
Subject: Re: [MW:25676] Tube to Tubesheet Joint
Taking into account that your Pno is 43 you may benefit of the provisions of QW 202.4.
However before take a final decisions check the requirements of QW 202.6
2016-11-12 16:23 GMT+02:00 'prem_nautiyal26' via Materials & Welding <material...@googlegroups.com>:
Hi
Assuming your construction code is ASME SEC VIII div.1,
You will have to carry out a separate tube to tube sheet mock up qualification.
Refer ASME SEC IX and SEC VIII Div 1 for details.
Also tube to Tube sheet mock up qualification will be mentioned in your approved QAP
REGARDS
PREM NAUTIYAL
9769316004
Sent from my Samsung Galaxy smartphone.
-------- Original message --------
From: pankaj phuse <pankaj...@gmail.com>
Date: 11/11/2016 16:15 (GMT+05:30)
To: Materials & Welding <material...@googlegroups.com>
Subject: [MW:25662] Tube to Tubesheet Joint
Dear Experts,
Need your guidance on the following:
We have tube to tube-sheet joint having Groove + Fillet Weld without grooves & expansion. (Tube-2.7mm, Tubesheet-45mm, P No.43 to P. No.43)
I have PQR qualified on plate 10mm Thk. (P No.43 to P No.43, Qualification Range - 1.5 to 20mm).
Can I use the same WPS for this joint or we have to qualify new procedure.
Procedure qualified as per ASME Sec.IX.
Need clarification with reference to clause number.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-weld...@googlegroups.com.
To post to this group, send email to
material...@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/a0bf2487-921c-40df-a1f4-cc6886e07182%40googlegroups.com.
For more options, visit
https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-weld...@googlegroups.com.
To post to this group, send email to
material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3vk1jfblmfkop6qg13yd2on8.1478960138453%40email.android.com.
For more options, visit
https://groups.google.com/d/optout.
--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-weld...@googlegroups.com.
To post to this group, send email to
material...@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CAPOi40CvE1uMPy%3D9tkh3nNYYM1LCpvxobZhbQWbZivqGgJXMXA%40mail.gmail.com.
No. You cannot use 10.0mm PQR for tube to tubes heel joint.
Minor adjustment - ASME Section VIII Div. 1 does not mandate tube-to-tubesheet mockup for qualification - however Division 2 does.
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of George Dilintas
Sent: Sunday, November 13, 2016 7:28 AM
To: Meghanadh K
Subject: Re: [MW:25676] Tube to Tubesheet Joint
Taking into account that your Pno is 43 you may benefit of the provisions of QW 202.4.
However before take a final decisions check the requirements of QW 202.6
2016-11-12 16:23 GMT+02:00 'prem_nautiyal26' via Materials & Welding <materials-welding@googlegroups.com>:
Hi
Assuming your construction code is ASME SEC VIII div.1,
You will have to carry out a separate tube to tube sheet mock up qualification.
Refer ASME SEC IX and SEC VIII Div 1 for details.
Also tube to Tube sheet mock up qualification will be mentioned in your approved QAP
REGARDS
PREM NAUTIYAL
9769316004
Sent from my Samsung Galaxy smartphone.
-------- Original message --------
From: pankaj phuse <pankaj...@gmail.com>
Date: 11/11/2016 16:15 (GMT+05:30)
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:25662] Tube to Tubesheet Joint
Dear Experts,
Need your guidance on the following:
We have tube to tube-sheet joint having Groove + Fillet Weld without grooves & expansion. (Tube-2.7mm, Tubesheet-45mm, P No.43 to P. No.43)
I have PQR qualified on plate 10mm Thk. (P No.43 to P No.43, Qualification Range - 1.5 to 20mm).
Can I use the same WPS for this joint or we have to qualify new procedure.
Procedure qualified as per ASME Sec.IX.
Need clarification with reference to clause number.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a0bf2487-921c-40df-a1f4-cc6886e07182%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3vk1jfblmfkop6qg13yd2on8.1478960138453%40email.android.com.
For more options, visit https://groups.google.com/d/optout.
--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40CvE1uMPy%3D9tkh3nNYYM1LCpvxobZhbQWbZivqGgJXMXA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/MWHPR03MB281676B9A3440FA3FA7F050EA1BC0%40MWHPR03MB2816.namprd03.prod.outlook.com.
Your Code basis for that comment? Opinions don’t matter – cite the Code basis.
From: material...@googlegroups.com [mailto:material...@googlegroups.com]
On Behalf Of Shaunak Upadhyay
Sent: Monday, November 14, 2016 6:12 PM
To: material...@googlegroups.com
Subject: RE: [MW:25695] Tube to Tubesheet Joint
No. You cannot use 10.0mm PQR for tube to tubes heel joint.
On 15 Nov 2016 02:07, "John Henning" <jhen...@deltak.com> wrote:
Minor adjustment - ASME Section VIII Div. 1 does not mandate tube-to-tubesheet mockup for qualification - however Division 2 does.
From:
material...@googlegroups.com [mailto:material...@googlegroups.com]
On Behalf Of George Dilintas
Sent: Sunday, November 13, 2016 7:28 AM
To: Meghanadh K
Subject: Re: [MW:25676] Tube to Tubesheet Joint
Taking into account that your Pno is 43 you may benefit of the provisions of QW 202.4.
However before take a final decisions check the requirements of QW 202.6
2016-11-12 16:23 GMT+02:00 'prem_nautiyal26' via Materials & Welding <material...@googlegroups.com>:
Hi
Assuming your construction code is ASME SEC VIII div.1,
You will have to carry out a separate tube to tube sheet mock up qualification.
Refer ASME SEC IX and SEC VIII Div 1 for details.
Also tube to Tube sheet mock up qualification will be mentioned in your approved QAP
REGARDS
PREM NAUTIYAL
9769316004
Sent from my Samsung Galaxy smartphone.
-------- Original message --------
From: pankaj phuse <pankaj...@gmail.com>
Date: 11/11/2016 16:15 (GMT+05:30)
To: Materials & Welding <material...@googlegroups.com>
Subject: [MW:25662] Tube to Tubesheet Joint
Dear Experts,
Need your guidance on the following:
We have tube to tube-sheet joint having Groove + Fillet Weld without grooves & expansion. (Tube-2.7mm, Tubesheet-45mm, P No.43 to P. No.43)
I have PQR qualified on plate 10mm Thk. (P No.43 to P No.43, Qualification Range - 1.5 to 20mm).
Can I use the same WPS for this joint or we have to qualify new procedure.
Procedure qualified as per ASME Sec.IX.
Need clarification with reference to clause number.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-weld...@googlegroups.com.
To post to this group, send email to
material...@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/a0bf2487-921c-40df-a1f4-cc6886e07182%40googlegroups.com.
For more options, visit
https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-weld...@googlegroups.com.
To post to this group, send email to
material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3vk1jfblmfkop6qg13yd2on8.1478960138453%40email.android.com.
For more options, visit
https://groups.google.com/d/optout.
--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-weld...@googlegroups.com.
To post to this group, send email to
material...@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CAPOi40CvE1uMPy%3D9tkh3nNYYM1LCpvxobZhbQWbZivqGgJXMXA%40mail.gmail.com.
For more options, visit
https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-weld...@googlegroups.com.
To post to this group, send email to
material...@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/MWHPR03MB281676B9A3440FA3FA7F050EA1BC0%40MWHPR03MB2816.namprd03.prod.outlook.com.
For more options, visit
https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-weld...@googlegroups.com.
To post to this group, send email to
material...@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CAD1AzTQzozVFNp05ThrFSEKD_0KLqwn-SAKgTLMhL7WsGrEXaQ%40mail.gmail.com.
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:25662] Tube to Tubesheet Joint
Dear Experts,
Need your guidance on the following:
We have tube to tube-sheet joint having Groove + Fillet Weld without grooves & expansion. (Tube-2.7mm, Tubesheet-45mm, P No.43 to P. No.43)
I have PQR qualified on plate 10mm Thk. (P No.43 to P No.43, Qualification Range - 1.5 to 20mm).
Can I use the same WPS for this joint or we have to qualify new procedure.
Procedure qualified as per ASME Sec.IX.
Need clarification with reference to clause number.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a0bf2487-921c-40df-a1f4-cc6886e07182%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3vk1jfblmfkop6qg13yd2on8.1478960138453%40email.android.com.
For more options, visit https://groups.google.com/d/optout.
--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40CvE1uMPy%3D9tkh3nNYYM1LCpvxobZhbQWbZivqGgJXMXA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/MWHPR03MB281676B9A3440FA3FA7F050EA1BC0%40MWHPR03MB2816.namprd03.prod.outlook.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAD1AzTQzozVFNp05ThrFSEKD_0KLqwn-SAKgTLMhL7WsGrEXaQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/MWHPR03MB2816AE26B8D89A5A90BAC9EDA1BF0%40MWHPR03MB2816.namprd03.prod.outlook.com.To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.