Welders Repair Rate.

38 views
Skip to first unread message

Eseosa Agho Otoghile

unread,
Apr 16, 2024, 11:20:40 AM4/16/24
to Materials & Welding
Can I use the number joints failed as against the number of joint shot for repair rate .. further more the RT is 100%

Best Regards,

Eseosa 

Vikas Bhandari

unread,
Apr 16, 2024, 10:11:42 PM4/16/24
to material...@googlegroups.com
Depends on the client.
Some go by length of weld inspected and length of defect to get repair rate

--