Clarification of SA572 Cu content.

44 views
Skip to first unread message

Biplab Pal

unread,
Apr 18, 2015, 2:57:45 AM4/18/15
to materials-welding
Dear Experts,

I have a doubt of the interpretation of SA572
I chemical analysis it states "A Copper when specified shall have a minimum content of 0.20% by heat analysis (0.18% by product analysis)."

I want to interpret the meaning of specified. Is it PO or MTC.

My case is, contractor has purchased the material of structural steel. Their PO dose not mentioned that certificate need to me mentioned about Cu content, but in Lab test certificate the % of Cu is mentioned and it comes below the minimum requirement. The material shall be accepted or rejected.

Can you please clarify the matter.
I am expecting your valuable input and reply.

--
Thanks & Regards
Biplab Pal
Welding Inspector
E-mail:   bipla...@gmail.com
 
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
 

Ramin Kondori

unread,
Apr 18, 2015, 3:23:23 AM4/18/15
to material...@googlegroups.com
it's the PO

Best Regards

Ramin Kondori

Sr. QA/QC engineer

Yadavaran Oilfield Project

SIPC (SINOPEC)


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFnzQg0on-_jtshy7rkaGpQdiBD55t8q7FUtQZuu%3DDpcZy%2Bdmg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

pgoswami

unread,
Apr 18, 2015, 8:36:07 AM4/18/15
to material...@googlegroups.com, bipla...@googlemail.com
Hi Biplab,
 
Please below the scope of this steel as indicated in SA 572. Also refer the attached data sheet. Generally this steel is used in bridge construction or transmission towers, where weathering resistance is important. Presence of copper helps in that.
 
What would be the application of the steel in this case ?? If for outdoor application then presence of copper would be beneficial as stated previously. Accordingly the PO should be written or modified as required.
 
Appreciate your response.
 
Thanks.
 
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Engineer/Specialist
Ontario, Canada
 

 

Scope

This specification covers five grades of high strength low-alloy structural steel shapes, plates, sheet piling,and bars. Grades 42 [290], 50 [345], and 55 [380] are intended for riveted, bolted, or welded structures. Grades60 [415] and 65 [450] are intended for riveted or bolted construction of bridges, or for riveted, bolted, or welded construction in other applications



From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of Biplab Pal
Sent: Saturday, April 18, 2015 2:28 AM
To: materials-welding
Subject: [MW:23127] Clarification of SA572 Cu content.

--
SAS_A-572_HY-80_HY-100.pdf

george....@gr.bureauveritas.com

unread,
Apr 18, 2015, 9:10:19 AM4/18/15
to pgoswami, bipla...@googlemail.com
Cu us helping on grain refinement. It is increasing also the strength through precipitation in ferrite matrix. In higher amounts it can be detrimental. Therefore I wonder why there is no an upper limit

Sent from my BlackBerry 10 smartphone.
From: pgoswami
Sent: Σάββατο, 18 Απριλίου 2015 - 15:36
Subject: [MW:23130] RE: 23127] Clarification of SA572 Cu content.


For more options, visit https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

Biplab Pal

unread,
Apr 18, 2015, 11:46:44 AM4/18/15
to pgoswami, materials-welding
Dear Goswami,

This steel will be used for pipe structure in refinery construction. The area is not much corrosive.