Dear Sir,
I am confusing for EGW welder operator thickness qualified because we conduct test for welder operator on thickness 16.0 mm plates which are single pass only. As per ASME-IX QW-403.9 For single‐pass or multi pass welding in which any pass is greater than 1/2 in. (13 mm) thick, an increase in base metal thickness beyond 1.1 times that of the qualification test coupon. Can anyone clarify me maximum thickness qualified welder operator.
Regards
Anamul
QA/QC Engineer
It is restricted by the WPS only
best regards
Dr. Georgios Dilintas
Authorized Nuclear Inspector
Authorized Inspector Supervisor
I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS HELLAS A.E - PIRAEUS GREECE
Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
This message contains confidential information.
To know more, please click on the following link: http://disclaimer.bureauveritas.com