You can use as reference AWS D1.1:
· mild steel (yield strength up to 36 ksi [250 MPa])
· medium-strength steel (yield strength between 36 ksi and 65 ksi [250 MPa and 450 MPa])
· high-strength steel (yield strength between 65 ksi and 115 ksi [450 MPa and800 MPa])
--