Super Duplex (32205) To Copper Nickle 90/10 (SMAW + GTAW)

57 views
Skip to first unread message

Midhun murali

unread,
Aug 18, 2023, 6:00:10 AM8/18/23
to Materials & Welding
Dear Experts,

Can anyone tell me which Electrode and Filler wire should be used for Weld Between Super Duplex to Copper Nickles.

BR,
Midhun

james gerald

unread,
Aug 18, 2023, 9:07:10 AM8/18/23
to material...@googlegroups.com
Butter Super Duplex side with ERNi-1\ENi-1 and complete the Joint using ENiCu-7.

Thanks & Regards

J.Gerald Jayakumar




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/342c4e45-796c-43b9-ab8e-8131f2408cb8n%40googlegroups.com.

Vishwas Keskar Welding Manager WELDING

unread,
Aug 18, 2023, 9:07:10 AM8/18/23
to Materials & Welding
Pl. furnish below inf
1)What is type of joint 
2)What is service 
3)Operating temperature 

Midhun

unread,
Aug 19, 2023, 3:10:13 AM8/19/23
to material...@googlegroups.com
Please check the below

1)What is type of joint - Single V Butt Joint (Base Metal-1 SA 106 Gr B, With Cuni 90/10 Lining, Base Metal - 2  SA 790 S32205 Super Duplex)
2)What is service - SeaWater
3)Operating temperature - 50Deg.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Reply all