Hi,
I have made Welder Performance qualification with using P-no. 8 and F-no. 6.
Asme IX gives for welder qualification for: P-no. 1-15F; P-no. 34, and P-no. 41-49
Than he can weld Inconel Base metals
But F-no 6 gives for welder qualification for use only all F-no. 6.
F-no. 6 don't give for him permission for welding inconel filler materials
Am I correct?
What for the welder is given permission in welding Inconel materials but not with F-no 41-46???
Do someone can help with this misunderstanding?