In my condensing system my header line is having 2 materials
The line above sprayer which was connecting with condenser is SA 335 P11
And after sprayer till loop is SA 335 P91
Now my problem is whether we can weld or connect this SA 335 P11 and SA 335 P91 ?
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1897297439.973280.1434611732382.JavaMail.yahoo%40mail.yahoo.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3947C1F4AA7F42D392608CD31CE283A1%40homepg.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANGGvaJ0JZ-T2JkfHgz84iZZUCh4bHAx8L9PP2BJoKP1hhaVJQ%40mail.gmail.com.
Hi Arunkumar,You may follow this discussion and the provided solutions to your solve your problem. The table below provides overall electrode selection matrix for DMWs involving Grade-91 and other alloys.Thanks.Pradip Goswami, P.Eng,IWEWelding & Metallurgical Engineer/SpecialistOntario, Canada