WPS for SA387 Gr F11 CL2

18 views
Skip to first unread message

uday prabhu

unread,
Nov 6, 2021, 9:50:22 AM11/6/21
to Materials & Welding
Dear All,

Can someone give me WPS for SA387 Gr F11 CL2
Thickness : Shell 30mm & dished end 35mm
PWHT required as per code.
3mm SS.304 cladding from inside.

Regards,

Uday