Hi Mr Pinaki Boxi.
Production test coupons are mandatory as per ASME Sec- VII DIV-2. Please see the generic comparison of the ASME Sec –VIII codes in the following attachment (downloadable at the following web link).
The simulation test gives confidence about the materials , not after fabrication. Hence vessel test coupons are required.
Please look through following DIV-2 clauses with respect Test coupon requirements (with bullets as below).
Thanks..
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Engineering Specialist
Hamilton, Ontario, Canada
ca.linkedin.com/pub/pradip-goswami/5/985/299
http://www.impactrm.com/glossary/ref/ASME_Section_VIII_Comparison.pdf
From:
material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of Pinaki Boxi
Sent: Tuesday, October 20, 2015
10:10 AM
To: Materials & Welding;
Biplab Pal; chandan.majumdar
Subject: [MW:23760] PTC(Production
Test Coupon) Requirements.
Dear Sir/Experts,
We are going to the manufacturing the Sphere for Liquid/unsaturated LPG.Design Code ASME Section -Vlll Div-2, design temperature -34 deg centigrade. Materials are impacted tested at -34 deg centigrade wıth simulated heat treatment. Condition.
I have doubt regarding PTC. As per Section Vlll Div-1 if materials are under impact tested in that case PTC is mandatory.
But as per ASME Section Vlll Div-2 it is required or not please advised me with supporting clause/documents.
--
Thanks & Regards
Pinaki Boxi.
*Manager QA/QC*
*ARP Project Site, Turkey*
*Mob :- +905351054384.
--
You received this message because you are subscribed to the Google Groups
"Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email
to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOt02TCwCpbYde3uSevpac%3D8m-HSVO4MdP62%3DQ8D7nvHp6Tnhg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2F0EEE32404647B0BB537333AC86F436%40homepg.
For more options, visit https://groups.google.com/d/optout.