SUPPORT WELDING BY A PIPE WELDER

53 views
Skip to first unread message

NIKHIL THOMAS JOY

unread,
Nov 1, 2020, 5:37:24 AM11/1/20
to Materials & Welding

Dear Experts,

Greetings of the day,

If I qualified a welder in pipe 6”NPS material C.S (A106 Gr. B) with welding process GTAW+SMAW as per ASME SEC IX.

Can he weld the pipe support(Shoe ,Guide , trunnion support) of SMAW only & structural connections such as Gusset plate, bottom plate, bracings of material  A36  by using SMAW Process.

 

Experts please give answer.

anand gupta

unread,
Nov 1, 2020, 10:25:04 PM11/1/20
to material...@googlegroups.com

Dear

As per code WPS for butt joint it will qualify for all fillet.
Your welding is all fillet so you can weld.

Regards
Anand gupta
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bf0a7f55-b41a-469f-b9aa-577f730f7c63n%40googlegroups.com.

GENE MATSKO

unread,
Nov 1, 2020, 10:25:21 PM11/1/20
to material...@googlegroups.com
Yes, of course.

Gene Matsko


--

Manikandan J

unread,
Nov 1, 2020, 10:25:21 PM11/1/20
to material...@googlegroups.com
Yes he can weld by smaw process, without changing other essential variables. 

Regards, 
Manikandan. 



--