Calibration of Viewer for interpretation of Radiography film

507 views
Skip to first unread message

Manish Kumar

unread,
Oct 11, 2020, 3:04:04 AM10/11/20
to material...@googlegroups.com
Dear Sir,
As per technically, Is Calibration of radiography film viewer need/requirement for interpretation of  radiography film as per ASTM section V article 2, T-234 ASTM 1390-12,ASTM E 1742 ?

Please advise in this concern.                                                                    
Enclo-
Reference documents is attached for ASTM terminology.
--
Regards

Manish Kumar
Inspection(Mechanical) Engineer
PDIL-HURL Barauni site
astm.jpeg
astm 1.jpeg

George Dilintas

unread,
Oct 11, 2020, 10:27:53 PM10/11/20
to material...@googlegroups.com
No there is no viewer's calibration requirmenet

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHfQ4k48w_%2BXOrPnU_YP2Eg4N8cRcgWhjrXXjm_vXeTyB2p5OA%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

james gerald

unread,
Oct 11, 2020, 10:50:12 PM10/11/20
to material...@googlegroups.com
but only Darkness level to be maintained as recommended and Lux meter to be calibrated.

Thanks & Regards

J.Gerald Jayakumar




Regino Millan

unread,
Oct 11, 2020, 11:00:59 PM10/11/20
to material...@googlegroups.com
Agreed no Viewer calibration requirements 
--
Best Regards

Regino millan