Benaouda Mezrar

ungelesen,
10.02.2022, 05:29:3910.02.22
an Materials & Welding
HI friend 
in wich code i can find the metal API 5LC gr LC65-2205 ? (API SPECEFICATION 5L or table QW/QB-422 of ASME IX)
could any one help me please 
thanks  

james gerald

ungelesen,
10.02.2022, 22:16:2010.02.22
an material...@googlegroups.com
Please check API5LC, an old edition attached.

Thanks & Regards

J.Gerald Jayakumar




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/218d1f82-f407-452a-b84f-820796e594a9n%40googlegroups.com.
API SPEC 5B-2008.PDF

vijay

ungelesen,
29.03.2022, 03:47:2929.03.22
an material...@googlegroups.com

Benaouda,


Please refer to API 5LC code for Gr. LC65-2205 (UNS S31803).

Regard,
Vijay

--
Allen antworten
Antwort an Autor
Weiterleiten