UNPAINTED WELDED JOINTS IN HISTROSTATIC TESTING OF TANKS

22 views
Skip to first unread message

AGUSTIN JIMENEZ

unread,
Mar 18, 2015, 7:02:23 AM3/18/15
to materials welding
Good morning COLLEAGUES AM 2 MONITORING THE MANUFACTURE OF TANKS AND THE POINT OF HYDROSTATIC TEST OF LEAK OR HAVE CARRIED OUT THE PROBLEM REQUIRING UNPAINTED WELDED JOINTS, WHERE I'M LOOKING FOR STANDARDS IN ME SAY THAT? OR I CAN VACUUM TESTING AND / OR DIESEL ALL WELDING TO ENSURE THAT NO LEAKS? THANK YOUR VIEWS AND INSPECTORS ARE CERTIFIED SI API 653 OR OTHER RELATED TO PLACE THE NUMBER TO GIVE MORE SUPPORT RESPONSE THANKS
 
Agustin Jimenez

 

AGUSTIN JIMENEZ

unread,
Mar 19, 2015, 12:04:12 AM3/19/15
to material...@googlegroups.com
Hi.
I read API 650 but I not find information, i want know if i can or not do it the hidrostatic test of tank after paint all welds.
 
Agustin Jimenez

 



El Miércoles, 18 de marzo, 2015 6:30:45, 'AGUSTIN JIMENEZ' via Materials & Welding <material...@googlegroups.com> escribió:


Good morning COLLEAGUES AM 2 MONITORING THE MANUFACTURE OF TANKS AND THE POINT OF HYDROSTATIC TEST OF LEAK OR HAVE CARRIED OUT THE PROBLEM REQUIRING UNPAINTED WELDED JOINTS, WHERE I'M LOOKING FOR STANDARDS IN ME SAY THAT? OR I CAN VACUUM TESTING AND / OR DIESEL ALL WELDING TO ENSURE THAT NO LEAKS? THANK YOUR VIEWS AND INSPECTORS ARE CERTIFIED SI API 653 OR OTHER RELATED TO PLACE THE NUMBER TO GIVE MORE SUPPORT RESPONSE THANKS
 
Agustin Jimenez

 
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2019460376.1022370.1426676445127.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.


Reply all
Reply to author
Forward
0 new messages