Relation between diffusible hydrogen and welding current

40 views
Skip to first unread message

Pravin G

unread,
Jun 27, 2016, 7:36:04 AM6/27/16
to 'Agustin Jimenez' via Materials & Welding
Dear expert,

What is the correlation between diffusible hydrogen and welding current.

How does Welding current affects diffusible hydrogen ? Based on any specific code or theory?

Kindly help to explain.

Pravin Poornachandran
Singapore
Sent from my iPhone

George Dilintas

unread,
Jun 28, 2016, 2:12:14 AM6/28/16
to Meghanadh K


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5DFF92D3-8F9F-4BA9-A964-E41BEB02E7CA%40gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

prem_nautiyal26

unread,
Jun 28, 2016, 2:12:24 AM6/28/16
to material...@googlegroups.com

There is no relation between diffusible hydrogen content and Welding current.



Sent from my Samsung Galaxy smartphone.

dili...@gmail.com

unread,
Jun 28, 2016, 7:21:19 AM6/28/16
to 'prem_nautiyal26' via Materials & Welding
Research papers demonstrate the contrary

Sent from my BlackBerry 10 smartphone.
From: 'prem_nautiyal26' via Materials & Welding
Sent: Τρίτη, 28 Ιουνίου 2016 - 09:12
Subject: Re: [MW:25017] Relation between diffusible hydrogen and welding current

Pravin G

unread,
Jun 28, 2016, 11:39:30 PM6/28/16
to material...@googlegroups.com
Dear George,

Thank you very much for the document shared. It's very useful.

Pravin Poornachandran


Sent from my iPhone

Kannayeram Gnanapandithan

unread,
Jun 28, 2016, 11:40:34 PM6/28/16
to materials-welding

Yes, diffusible hydrogen is more, more arc voltage is required to push the current due to bad conduct electricity by Hydrogen. Example 6010 is required more arc voltage when compared with 7018