Dear all,
I know that 100mm is permissble distance between two consecutive longitudinal seams but, can any one confirm minimum distance between two longitudinal seams should be mantained. Kindly mention ASME clause.
Thanks &Regards
Gurunath Hanamar
Section VIII-1 UW(9)(d): except when the longitudinal joints are radiographed 100 mm each side of each circumferential welded intersection, vessels made up of two or more courses shall have the centers of the welded longitudinal joints of adjacent courses staggered or separated by a distance of at least five times the thickness of the thicker plate
best regards
Dr. Georgios Dilintas
Authorized Nuclear Inspector
Authorized Inspector Supervisor
API 510 Inspector
I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE
Tel: +30 210 40 63 113/4
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
"Gurunath.Hanamar" <guru...@gmail.com>
Sent by: material...@googlegroups.com 14/06/2012 06:24
|
|
Thanks &Regards
Gurunath Hanamar
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~
NOTICE: This message contains information which is confidential and the copyright of our company or a third party. If you are not the intended recipient of this message please delete it and destroy all copies. If you
are the intended recipient of this message you should not disclose or distribute this message to third parties without the consent of our company. Our company does not represent, warrant and/or guarantee that the integrity of this message has been maintained nor that the communication is free of virus, interception or interference. The liability of our company is limited by our General Conditions of Services.
Nota : Ce message contient des informations confidentielles propriété de notre société et/ou d'un tiers. Si vous n’êtes pas parmi les destinataires désignés de ce message, merci de l'effacer ainsi que toutes ses copies. Si vous êtes parmi les destinataires désignés de ce message, prière de ne pas le divulguer ni de le transmettre à des tiers sans l’accord de notre société. Notre société ne peut garantir que l’intégrité de ce message a été préservée ni que la présente communication est sans virus, interception ou interférence. La responsabilité de notre société est limitée par nos Conditions Générales de Services.
~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
Hello To ALL,This clause applicable to Pressure Vessel, What about PIPING can any one suggest for piping as per (API 1104, B31.4, B31.3 or B31.1).Thanks.
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
| Such stuff are referenced in corresponding project specifications, as these can not be generalised. |
ವಂದನೆಗಳೊಂದಿಗೆ / Best regards, |
Nandesh Kumar A Abu Dhabi, UAE P.S. : Please don't print this e-mail unless you really need to. --- On Thu, 28/3/13, Himanshu Patel <absg...@gmail.com> wrote: |
HELLO,
| From: Ritixa Tandel Sent: Δευτέρα, 21 Μαρτίου 2016 - 12:27 To: Materials & Welding Reply To: material...@googlegroups.com Subject: Re: [MW:24562] Distance between two L-Seam |
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20160331135534.6729814.90184.2438%40gmail.com.
HELLO,I AM STUDYING & REFERRING ABOUT DESIGN OF EQUIPMENT.CONTINUE TO YOUR DISCUSSION ABOUT ''DISTANCE BETWEEN TWO L-SEAM''........WHAT SHOULD BE THE MINIMUM DISTANCE IF MY REACTOR IS LIKE THIS:--SS 316 L REACTOR (3 KL WORKING CAPACITY)--SHELL: 1500 MM ID x 1700 MM LG x 8 MM THK--REACTOR WITH DOUBLE LIMPET COIL.REGARDS RITIXA.ANKLESHWAR, GUJARAT. INDIA.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7750e6fe-212b-40ed-945e-9d1d8b6c309f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
EN 13445-4:2009
6.2 Vessels or parts made of more than one course
Where a vessel or vessel part is made of two or more courses the longitudinal weld joints of adjacent courses shall be staggered by 4 e with 10 mm minimum, or 30 mm minimum when the vessel or vessel part is either working in the creep range or designed by Design by Analysis – Direct Route (Annex B of EN 13445-3:2009) or designed using 6.3 of EN 13445-3:2009.
Pl refer uw9 D
On Thu, Apr 19, 2018 at 9:34 AM, udaya bhaskar<dus...@gmail.com> wrote:
My dear, distance between two L seams for pressure vessels minimum 250- 300mm.
On Mon 21 Mar, 2016, 15:57 Ritixa Tandel, <ritixat...@gmail.com> wrote:
HELLO,I AM STUDYING & REFERRING ABOUT DESIGN OF EQUIPMENT.CONTINUE TO YOUR DISCUSSION ABOUT ''DISTANCE BETWEEN TWO L-SEAM''........WHAT SHOULD BE THE MINIMUM DISTANCE IF MY REACTOR IS LIKE THIS:--SS 316 L REACTOR (3 KL WORKING CAPACITY)--SHELL: 1500 MM ID x 1700 MM LG x 8 MM THK--REACTOR WITH DOUBLE LIMPET COIL.REGARDS RITIXA.ANKLESHWAR, GUJARAT. INDIA.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7750e6fe-212b-40ed-945e-9d1d8b6c309f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Saygılarımla / Regards
Tuğrulhan ÖZDEMİR
API 653 AI, Welding & Materials Eng.
ASNT VT, PT, MT, RT L-II
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/