Dear experts,
I had a problem while testing SS electrodes on Non-magnetic eccentricity machine, when placing electrode into the sensing probes it shows the needle deflection of 20 divisions on both sides which indicates non ecentricity and probably tapered burning will arise when welding it, but when actually welding that electrode it does not show any sign of Tapered burnin.
Would be thankful if someone could explain me why this is happening and how to fix it,
Regards