Dear Experts 

I am new for this job please help me 

for PQR of LTCS

1) required thickness min is 6.35mm &  dia is 12 inch

2) design press = 20kg/cm2
    design temp  = -45.6/37.8 degreee celcius
     op press      = 20 max
     op temp       = -40 degree celcius

3)  material is pipe - A 333 GR 6(P1 &G1) and flange - A350 GR LF2 RF

4) service is LPG plant- Relief and blow down

now please suggest me 
 a) what is is the size of the test coupon can be selected(dia with schd) where can i find the exact length of weld required to carry out mechanical testing for this PQR?
 b) is it possible to carry out the PQR for pipe to flange joint 
 c) what consumable can be selected for this if GTAW & SMAW ?
 

Regards
AHMAD

Himan Nikdin

unread,
Sep 8, 2016, 3:20:56 AM9/8/16
to material...@googlegroups.com
Hi buddy!!!

Since your joint is between P.No 1-Gr No 1 (A333-Gr6) and P.No1-Gr No2 (A350 LF2) and impact test is mandatory (cause Gr No to be essential variable) so your PQR shall joint between P.No 1-Gr No 1 & P.No1-Gr No2. I think most available material to meet above-mentioned criteria is SA-516Gr70 to SA-516Gr60.

your quarries;
a) If you do not have other thicknesses so thickness 10mm is so enough!.
b)Yes.
c)GTAW filler; ER-80SNi(if NACEMR0175/ISO15156 is not applicable)/SMAW filler: E7018-1.

Regards,
Himan Nikdin


Date: Wed, 7 Sep 2016 22:21:03 -0700
From: must...@gmail.com
To: material...@googlegroups.com
Subject: [MW:25350] LTCS PQR
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1dff4f26-85ba-4a9d-a731-d037ac27bea3%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

TDK YOKESH

unread,
Sep 8, 2016, 3:21:09 AM9/8/16
to material...@googlegroups.com

Dear Ahmad ,

The main difference between LTCS and Carbon manganese steel is the percentage of manganese , silicon and nickel which is pretty high in LTCS. LTCS weldability is similar to CS except it may require preheat , PWHT , hardness check as it mostly operates at low temp .  You can use low hydrogen electrode ( E7018 ) and ER70S6 . Check for heat treatment and impact toughness requirements  as per your project specification and do the necessary with your PQR .

Thanks
TDK Yokesh


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

Babur Khan

unread,
Sep 8, 2016, 3:21:33 AM9/8/16
to material...@googlegroups.com
Dear Mr. Mushtaq Ahmad,
Please clear following points.
1) Qualification Code.
2) Thickness range (Min. Max.)
Client requirements (Saudi Aramco etc) 

Regards,

Muhammad Babur Khan Lashari
Sr. QA/QC Inspector

(CSWIP 3.1 / CWI II From PWI) 

 Khaled Juffli Industial Company

Mob: + 966 56 2179280 / 58 2774568

PAK : + 92 334 6186285

Skype: babur.lashari

E-Mail: babur...@kjgroup.com


--

Himan Nikdin

unread,
Sep 8, 2016, 6:47:32 AM9/8/16
to material...@googlegroups.com
ER70S-6 can not be used, because impact test limitation.

Regards,
Himan Nikdin

Sent from my iPhone

Mustaq Ahmad

unread,
Sep 10, 2016, 12:30:42 AM9/10/16
to Materials & Welding
1) Code is B31.3 

2) thickness is min  6.35mm only no other thickness

To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.

George Dilintas

unread,
Sep 13, 2016, 7:30:04 AM9/13/16
to Meghanadh K
in your case and assuming that your Code is ASME VIII-1,  A333 for this thickness & temperature  is not exempted from Impact test. What is the governing thickness of A350? You can avoid impact if you satisfy all conditions of UG-20 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
Reply all
Reply to author
Forward
0 new messages