Kindly let me know the filler wire to be used for welding SA 240 TP 304 to SA 276 TP 310 material & SA 276 TP 310 to SA 276 TP 310 Material
Thanks & Regards,
Prashant Panchal
Hi Marvin,
Please refer your Client Specification, if it's not there refer your project or Client approved "Piping Material Specification " (PMS) for MDMT.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/D9EA8DC3-B050-49CA-8706-B751739B0B3C%40yahoo.com.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/D9EA8DC3-B050-49CA-8706-B751739B0B3C%40yahoo.com.
For more options, visit https://groups.google.com/d/optout.
Best Regards
Muhammad Ishtiaq
Saudi Aramco PID (ABSG),
Naphtha processing & Aromatics Complex
RFP-66,Package-12
Jizan Refinery-KSA
Dear all,
Kindly let me know the filler wire to be used for welding SA 240 TP 304 to SA 276 TP 310 material & SA 276 TP 310 to SA 276 TP 310 Material
Thanks & Regards,
Prashant Panchal
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/D9EA8DC3-B050-49CA-8706-B751739B0B3C%40yahoo.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/BL2PR17MB0833E556E9F0809143B645C4C3470%40BL2PR17MB0833.namprd17.prod.outlook.com.
can we use ER 309 filler wire for welding SA 240 TP 304 to SA 276 TP 310.
& ER 347 filler wire for welding SA 276 TP 310 to SA 276 TP 310.
Regards,
Prashant Panchal
can we use ER 309 filler wire for welding SA 240 TP 304 to SA 276 TP 310.
& ER 347 filler wire for welding SA 276 TP 310 to SA 276 TP 310.
Regards,
Prashant Panchal
From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> on behalf of Kannayeram Gnanapandithan <kgpan...@gmail.com>
Sent: Saturday, February 11, 2017 12:33:33 PM
To: materials-welding
Subject: Re: [MW:26038] Filler wire for welding SA 240 TP 304 to SA 276 TP 310 Mateial
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePTL0HcNS4Z3qTa64cO%3Dw27WjkFke3KSE%3DsRskfWWgKSA%40mail.gmail.com.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/BL2PR17MB08336C44D3CE01CD635A9FE8C3470%40BL2PR17MB0833.namprd17.prod.outlook.com.
Dear expert,
What is the required minimum temperature for piping {ei. Carbon steel pipe} to do impact test and please let me know where i can get this standard.
Regrds
MERVIN
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to www.rediffmail.com/cgi-bin/red.cgi?red=javascript:;&rdf=BT1VIlUmA24GLgcMBDVXYlt6UTQLJAdqVGU=" on-click="_e(event, 'cvml', 'materials-weld...@googlegroups.com')" target='_blank' rel=external>materials-weld...@googlegroups.com.
To post to this group, send email to www.rediffmail.com/cgi-bin/red.cgi?red=javascript:;&rdf=VGwEcwNwVzoCKgYNUGEDNlFwUDUKJQNuWGk=" on-click="_e(event, 'cvml', 'material...@googlegroups.com')" target='_blank' rel=external>material...@googlegroups.com.
To view this discussion on the web visit https:roups.google.com/d/msgid/materials-welding/D9EA8DC3-B050-49CA-8706-B75173...@yahoo.com.
For more options, visit https://groups.google.com/d/optout.
Best Regards
Muhammad Ishtiaq
Saudi Aramco PID (ABSG),
Naphtha processing & Aromatics Complex
RFP-66,Package-12
Jizan Refinery-KSA