Welder Qualification

58 views
Skip to first unread message

Ludmila MANUEL

unread,
Feb 9, 2015, 3:06:51 AM2/9/15
to material...@googlegroups.com

Dear experts,

 

Please can you give me your advise

 

Can I accept a job in process (Process piping) ASME B31.3 and spec ask for welder qualification as per ASME IX and the welder is qualified as API 1104 (Pipelines)

 

Is there any restriction?

 

thanks

 

 

Ludmila MANUEL

QC Inspector

TOTAL E&P ANGOLA

DT/EPT/ MHSAQ/QUA
Tel : +244 222 67 3443

Cell:+244 912 641 670
Email:
ludmila.Manuel@total.com

 trait (logo).jpg

logo.jpg

Mailing Address:

TOTAL E&P Angola
Rua 6 IL 6 B.I SONILS, Boavista Office B.I 100-01
1
Luanda - Angola

 

 

meisam shokri arfaei

unread,
Feb 9, 2015, 3:31:27 AM2/9/15
to material...@googlegroups.com
The first and main document should be used as a reference is a contract. If it mentioned in the contract documents, there is no problem. You will find the acceptable codes, standards, specs., procedures and any other guideline in those documents.

But generally in case of any conflict, the procedure cancels the spec, and the spec cancels the code or standard. Because the procedures have more details and adaptation compare to specs and specs also have more details and adaptation compare to codes and standards.

Regards

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1B0224B9A78AB34285E27B011195A0469E7D829F26%40AOEPTTA-EG11.main.glb.corp.local.
For more options, visit https://groups.google.com/d/optout.



--
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer





raouf salhi

unread,
Feb 9, 2015, 4:13:00 AM2/9/15
to material...@googlegroups.com
Dear Sir;

You should ask your client first or check the contract but usually this welder must be qualified according ASME IX.

Regards
 
SALHI Raouf
QA/QC Engineer

Tel: Morocco +212628979891
      Tunisia +21621458258