Dear All
As per ASME SEC IX Nozzle branch connection Set on which thicknesss consider for ( Nozzle or main pipe)WPS & WQT selection 

Regards 
ELAVARASAN

venkateswara reddy Desireddy

unread,
Oct 18, 2025, 3:19:20 AM (yesterday) Oct 18
to material...@googlegroups.com
For set on joint branch pipe thickness should be taken for WPS. For WPQ branch OD and thickness essential variable. 

Regards 
D.V.Reddy


From: material...@googlegroups.com <material...@googlegroups.com> on behalf of Elavarasan Mech <elavaras...@gmail.com>
Sent: Saturday, October 18, 2025 7:51:28 AM
To: material...@googlegroups.com <material...@googlegroups.com>
Subject: [MW:35841] SET ON ASME SEC IX
 
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4ym7crHij%3DVpKu%3DGgwWENPN1j1fR%2BhZyZZGCC2-OkgTFWQ%40mail.gmail.com.

SENTHILKUMAR SWAMINATHAN

unread,
Oct 18, 2025, 3:19:20 AM (yesterday) Oct 18
to material...@googlegroups.com
Set ON - Nozzle
Set Thru - Shell

Thank you, 
Regards, 
S.SENTHILKUMAR


--

Vishwas Keskar

unread,
Oct 18, 2025, 6:20:26 AM (yesterday) Oct 18
to material...@googlegroups.com
Pl refer ASME SEC IX 
It enlists in detail qualification / limits 

--

james gerald

unread,
Oct 18, 2025, 12:59:51 PM (21 hours ago) Oct 18
to material...@googlegroups.com
For Set-on Nozzle,

For Base Metal Thickness consider shell/ reinforcement thickness welded to Nozzle Wall thickness.

For Weld metal Thickness (PWHT calculation) use below.

Inline image
Inline image

Inline image
Inline image
  For Weldolet connections see below.

Inline image
According ASME Sec.IX,

Inline image
Inline image

Thanks & Regards

J.Gerald Jayakumar

0091-8838619635



Ramamoorthi Thangarasu

unread,
Oct 18, 2025, 2:07:49 PM (20 hours ago) Oct 18
to material...@googlegroups.com
Hi

Set In  mostly used for High pressure system it's considered mother pipe thickness only (bevel to be make only mother pipe)WPS and WQT selection to be select mother pipe.

Note if Set On Fillet  weld only applicable,no need to check size and thickness.