Hydrostatic temp.

60 views
Skip to first unread message

sajid ahmad

unread,
Jul 4, 2015, 1:56:26 PM7/4/15
to material...@googlegroups.com

Dear experts
What is the maximum and minimum temperature to be allowed in order to hydrostatic/pneumatic test.
Regards
M.Sajid

Tamizh Selvan

unread,
Jul 4, 2015, 11:44:25 PM7/4/15
to material...@googlegroups.com

Refer asme sec viii div 1 UG 99

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAKkJLcyL6Hvar%2BjkeG_Qx9qHiXtHSWRZYDfS76MO7CGFjPR1g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Prakash Gotimukul

unread,
Jul 5, 2015, 1:39:24 AM7/5/15
to materials-welding
Dear All,
Any topic that you raise, please give details of equipment/product and relevant code/standards that you are refering. This will make the topic easy to understand and elicit replies.After all we are interested in standard requirement, unless it is a open, general question.?

Rgds
G.Prakash
AIS, AIA LLC TX, USA

--

Jignesh Desai

unread,
Jul 7, 2015, 11:27:47 PM7/7/15
to material...@googlegroups.com, gprak...@gmail.com
If your question is related to ASME Sec VIII-Div I, then UG-99-(h) recommends as below

"The metal temperature during hydrostatic test be maintained at least 30°F (17°C) above the minimum design metal temperature, but need not exceed 120°F (48°C), to minimize the risk of brittle fracture."
Also the test liquid shall be at a temperature higher than the nil-ductility transition temperature of the material being tested.- Reference ASTM E1003.

The nil ductility temperature is the highest temperature at which a material experiences complete brittle fracture without appreciable plastic deformation.


Regds/Jignesh


On Sunday, 5 July 2015 11:09:24 UTC+5:30, Prakash Gotimukul wrote:
Dear All,
Any topic that you raise, please give details of equipment/product and relevant code/standards that you are refering. This will make the topic easy to understand and elicit replies.After all we are interested in standard requirement, unless it is a open, general question.?

Rgds
G.Prakash
AIS, AIA LLC TX, USA

On Sat, Jul 4, 2015 at 3:59 PM, sajid ahmad <sajid...@gmail.com> wrote:

Dear experts
What is the maximum and minimum temperature to be allowed in order to hydrostatic/pneumatic test.
Regards
M.Sajid

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages