Dear Experts
We have one project, Material is Alloy P22, A335 (Cr2.25 and Mo 1), Customer requirement
" where heat treatment of low alloy steel is required the weld joint shall be immediately heat treated without allowing it to cool below 150C (300F). if this is not practical the weld and adjacent pipe shall be uniformly heated to min 300C (570F), kept for 20 minutes , wrapped with insulation allowed to cool and heat treated later"
Please tell me what will be metallurgical affect in weld area if above condition will not follow, only maintain preheat temperature 200C during welding as per WPS/ PQR and conduct the PWHT after one or two days
Best Regards
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-weld...@googlegroups.com.
To post to this group, send email to
material...@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/936617816.5150279.1463694788989.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit
https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-weld...@googlegroups.com.
To post to this group, send email to
material...@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/20160523155102.6713426.4887.3069%40gmail.com.
For more options, visit
https://groups.google.com/d/optout.