Dear experts,

I'm writing WPS for overlay following ASME IX, but I have a concern about section QW 403.20 " If the chemical composition of the weld metal overlay is specified in the WPS, a change in the P-Number listed in Table QW/QB-422 to another P-Number or unlisted base metal, or a change in Group Number for P-No. 10 or P-No. 11 base metals.
If the chemical composition of the weld metal overlay is not specified in the WPS, qualification on P-No. 5A or any lower P-Number base metal also qualifies for weld metal overlay on all lower P-Number base metals".

I hope that you can help me to explain about this paragraph. If possible, please give me a specifc example. Thank you all!

james gerald

unread,
Apr 10, 2024, 3:13:43 AMApr 10
to material...@googlegroups.com
This clause is pertaining to substrate Base material (P.No.) over which weld overlay is Done.

Normally the Client specification or the mandate code will specify the chemistry of the overlay and at what depth from the Fusion line.

An example of Refinery code giving chemistry requirement in API RP-582 below.

Inline image

Hope now you can read and understand.

Thanks & Regards

J.Gerald Jayakumar

0091-8838619635



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/40c92c78-d955-4db9-bb71-14be4a366225n%40googlegroups.com.

Dương Vinh Quang

unread,
Apr 10, 2024, 10:24:53 AMApr 10
to material...@googlegroups.com
Thank you!
I don't understand how QW403-20 is different from QW403-11?

What does it mean for QW 403.20 to determine the chemical composition of the weld metal overlay specified in the WPS? Can you please explain clearly here? Is it possible to determine the chemical composition of the weld overlay in PQR after the overlay is completed? What is the method to determine it?

Thank you for your contribution!

Best ragards!
....................................
DƯƠNG VINH QUANG - WELDING ENGINEER
● Welding Team - Central Engineering - NSRP



Reply all
Reply to author
Forward
0 new messages