Hi Kalemullah,
MR-0175/ISO 15156 specifies that SSC/SOHIC testing should be done as per NACE TM-0177.This testing requirements are quite severe. You need to go through the results and try to seek the proper resolutions.
SOHIC testing on the PQR was originally called for in your project specifications??
Appreciate your response.
Thanks.
Pradip Goswami, P.Eng,IWE
Independent Welding & Metallurgical Engineering Specialist &
Consultant.
Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions w.r.t.
applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups
"Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email
to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20160413160528.13286.qmail%40f4mail-235-76.rediffmail.com.
For more options, visit https://groups.google.com/d/optout.
Hi Kalemullah,
MR-0175/ISO 15156 specifies that SSC/SOHIC testing should be done as per NACE TM-0177.This testing requirements are quite severe. You need to go through the results
SOHIC testing on the PQR was originally called for in your project specifications??
Appreciate your response.
Thanks.
Pradip Goswami, P.Eng,IWE
IndependentWelding & Metallurgical Engineering Specialist &
Consultant.
Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299
pgos...@quickclic.net
pradip....@gmail.com
From:
qama...@rediffmail.com [mailto:qama...@rediffmail.com]
Sent: Wednesday, April 13, 2016
12:05 PM
To:
material...@googlegroups.com
Subject: [MW:24682] SSC test
acceptance limit.
Dear Experts,
We are doing pipeline project for international client at UAE. We have completed
Now the PQR test conducted for the SSC test and SOHIC test.
But the test lab informed that linear indication was observed in two test specimen after 30 days SSC test.
Now the client instructed
Please suggest any acceptance criteria and resolution. Failure of the test will result huge impact on the 400 welded joints. Please suggest.
Pipeline Material:API 5L Gr.B X-60 as per shell standards.
Kalemullah
UAE-0569902364
Get your own FREE website, FREE domain
& FREE mobile app with Company email.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and
meant for educational applicable code/standard/contract documents.