There is no requirement or restriction in the Code for a minimum distance between 2 welds.
The Code is not a handbook, you have to implement basic metallurgy and sound engineering judgement
best regards
Dr. Georgios Dilintas
Authorized Nuclear Inspector
Authorized Inspector Supervisor
I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE
Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
This message contains confidential information.
To know more, please click on the following link: http://disclaimer.bureauveritas.com
| As per aramco std. Required min distance 25 mm or 3 times of wall thk whichever is greater. as per goog engg. Practice keep maximum distance. a p gupta |
|
|
|