i am preparing WPS and PQR for overlay for the first time. i have checked ASMEIX QW-453. it just confused me!!!!

actually we are finding which materials is the most suitable one for overlaying. the base metal is  A216 WCB and the overlay are 
stellite, monel, F316 and 13%Cr. 

i read that the dimentions of base metal should be 15*15 cm, with 2.5cm thickness. which examinations should be done on samples to prepare PQR? PT, chemical analysis, hardness nad macro? are these enough?

can somebody send me a sample of PQR and WPS for overlay please.
best regards
sara

SATISH SHAH

unread,
May 20, 2016, 10:51:28 PM5/20/16
to Materials & Welding
Dear

As per ASME Sec. IX, Table QW-453 there are two types of Overlay (1) Corrosion Resistance (2) Hard Facing. So, 1st you decide types of  Overlay and then follow notes no given in Table QW 453.

dili...@gmail.com

unread,
May 24, 2016, 5:40:41 AM5/24/16
to material...@googlegroups.com
What is the purpose of overlay? Hard facing or corrosion protection?

Sent from my BlackBerry 10 smartphone.
Sent: Τετάρτη, 18 Μαΐου 2016 - 07:34
To: Materials & Welding
Subject: [MW:24811] WPS and PQR for overlay

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/888a9a67-e8a7-4f15-b395-49cd80479b27%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Reply all
Reply to author
Forward
0 new messages