| You can refer to Caustic service graph given in API 571, Damage Mechanisms. It is given under topic of Caustic Embrittlement/caustic SCC. Carbon steel is widely used for this service, however at certain temperature MOC's are upgraded. thanks n regards, Nishant Nair Senior Engineer Reliability Sent from Yahoo Mail on Android
|