Dear Experts,
Greetings of the day.
Refering to SA 182 of ASME Sec. IIC Ed. 2013, SS 316 Electrodes are suggested for repair welding. Based on that may I use ER316/ ER316L filler wires for welding of SS 316Ti Base Metal? or ER318 shall be preferred?
Your expert's opinion on the above will be highly appreciated.
Thanks & regards,
C. R. GANDHI
HAMID HAMIDI
unread,
Jul 5, 2015, 8:25:38 AM7/5/15
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to material...@googlegroups.com
you can use of ER318 & ER316L.but ER318 is better.