Zihni Hakim

unread,
Aug 4, 2016, 3:15:25 AM8/4/16
to Materials & Welding
Hello,
Is there anyone know the material differences from ASTM A105 and A216 Gr.WCB?
because, if i've seen it based on the chemical and mechanical properties, they're all the same..
Anyone can tell, when we should use A105 or A216?

Nb : It is to be used for Plug Valve Material in pipeline engineering
Any help would be apreciated,
Thankyou


Best regard,
Zihni

Mostafa Kamel Hussein

unread,
Aug 4, 2016, 6:41:01 AM8/4/16
to material...@googlegroups.com
Dear Sir
Selection of material is only engineering scope NOT others. Selection of material is based on many parameters as service condition, MDMT, pressure required. if your engineering document has a specified material while you have equivalent one in your local market, then you should to raise concession request (CR) to your client for approval.


Regrds, 

 

 
 







Show original message
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsub...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6318ec8b-444b-4b70-aeec-8eedb4e6e4ab%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


Karthi Keyan

unread,
Aug 5, 2016, 10:27:58 PM8/5/16
to material...@googlegroups.com

Hi,

    A105 is forging material and A216 WCB is a casting material. I can suggest forging material is better than casting and also plug material will worn out during more operation. So you select A105.

Regards,

Karthikeyan


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

Alpesh Sakhreliya

unread,
Aug 5, 2016, 10:27:58 PM8/5/16
to 'Mostafa Kamel Hussein' via Materials & Welding

Hi ,

 

As per your mail, your application pipeline plug valve , both material is good , but size 2” and blow A105  and 4” and above A216 gr  availably in market

 Note : A105 mien’s this forge material   and A216 gr WCB casting material

 

 

Raged

Alpesh Sakhreliya

 

 

Sent from Mail for Windows 10

 

From: 'Mostafa Kamel Hussein' via Materials & Welding
Sent: Thursday, August 4, 2016 4:10 PM
To: material...@googlegroups.com
Subject: Re: [MW:25193] A105 vs A216 Gr. WCB

 

Dear Sir

Selection of material is only engineering scohipe NOT others. Selection of material is based on many parameters as service condition, MDMT, pressure required. if your engineering document has a specified material while you have equivalent one in your local market, then you should to raise concession request (CR) to your client for approval.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.


To post to this group, send email to material...@googlegroups.com.

George Dilintas

unread,
Aug 6, 2016, 6:11:35 AM8/6/16
to Meghanadh K
SA 216 IS FOR CASTINGS.
SA 105 IS FOR FORGINGS.
THERE ARE SOME KIND OF ITEMS THAT DUE TO SIZE AND SHAPE CAN NOT BE FORGED. 
SO THERE IS A NEED FOR A SPEC FOR CASTINGS AND FOR A SPEC FOR FORGINGS

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis