Need your advice for equivalent material flange with spec A 694 Grade F65. We need only 2 ea flange 2" but no available stock in market. we also have try to request manufacture but they decline since they have a minimum order. Your advice is highly appreciated. Thanks


Regards,


Lukman



Vijay Patre

unread,
Dec 24, 2016, 5:56:47 AM12/24/16
to material...@googlegroups.com
A694 F65 grade material is indicated in B 31.3, special material for high temp haigh pressure  service. End user can give you concurrence to use other material, since allowable stress indicated in 31.3 is much higher than the generally used CS material.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1328324844.1297699.1482489238938%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

mubeen mubeen

unread,
Dec 24, 2016, 10:34:45 PM12/24/16
to material...@googlegroups.com
Hi, You may select ASTM A707 F60 L3 as per 02-SAMSS-011, provided you should need to get approval from your customer.

Regards,
Mubeen

On Sat, Dec 24, 2016 at 1:54 PM, Vijay Patre <vijay....@gmail.com> wrote:
A694 F65 grade material is indicated in B 31.3, special material for high temp haigh pressure  service. End user can give you concurrence to use other material, since allowable stress indicated in 31.3 is much higher than the generally used CS material.

On Dec 24, 2016 8:17 AM, "'lukman hakim' via Materials & Welding" <materials-welding@googlegroups.com> wrote:
Dear Expert,


Need your advice for equivalent material flange with spec A 694 Grade F65. We need only 2 ea flange 2" but no available stock in market. we also have try to request manufacture but they decline since they have a minimum order. Your advice is highly appreciated. Thanks


Regards,


Lukman



--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1328324844.1297699.1482489238938%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages